(S)A240 S32900, (S)A240 TP 329, S32900 Stainless Plate, TP329

2015年7月30日 by admin

 

(S)A240 S32900, (S)A240 TP 329, S32900 Stainless Plate, TP329
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S32900, (S)A240 TP 329,
S32900 Stainless Plate, TP329 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S32900, (S)A240 S32900, S32900 Stainless plate,SS329, A240 329, SA240 329,TP329
 
What forms of A240 S32900 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S32900 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.08
1.00
0.040
0.030
0.75
23.0-28.0
Ni
Mo
N
Cu
Others
2.00-5.00
1.00-2.00
 
 
 

(S)A240 S32900 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRC
(S)A240 S32900
620
485
15
28

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                     
 

Tags: SA240 S32900  SA240 TP 329  S32900 Stainless Plate  TP329  