(S)A240 S31609, (S)A240 TP 316H, S31609 Stainless Plate, TP316H
2015年7月30日 by admin
(S)A240 S31609, (S)A240 TP 316H, S31609 Stainless Plate, TP316H
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31609, (S)A240 TP 316H,
S31609 Stainless Plate, TP316H as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S31609, (S)A240 S31609, S31609 Stainless plate,SS316H, A240 316H, SA240 316H,TP316H
What forms of A240 S31609 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S31609 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.04-0.10 | 2.00 | 0.045 | 0.030 | 0.75 | 16.0-18.0 |
Ni | Mo | N | Cu | Others | |
10.0-14.0 | 2.00-3.00 | | | |
(S)A240 S31609 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 S31609 | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.