(S)A240 S31008, (S)A240 TP 310S, S31008 Stainless Plate, TP310S

2015年7月30日 by admin

 

(S)A240 S31008, (S)A240 TP 310S, S31008 Stainless Plate, TP310S
 
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S31008, (S)A240 TP 310S,
S31008 Stainless Plate, TP310S as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S31008, (S)A240 S31008, S31008 Stainless plate,SS310, A240 310S, SA240 310S,TP 310S
 
What forms of A240 S31008 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S31008 Stainless Steel Overview
Stainless steel (S)A240 310/310S is an austenitic heat resistant alloy with excellent Resistance to oxidation under mildly cyclic conditions through 2000ºF. Its high Cr and Ni contents provide comparable corrosion resistance, superior resistance to oxidation and the retention of a larger fraction of room temperature strength than the common austenitic alloys like Type 304.
Stainless 310 is often used at cryogenic temperatures, with excellent toughness to -450°F, and low magnetic permeability.
 
As you can see below, Type 310S is a low carbon version of grade 310. 310S is less prone to embitterment  
and sensitization in service.
 
SS 310 Chemical Composition, %

C
Ni
C
Si
Mn
24.0-26.0
19.2-22.0
0.25 Max
1.50 Max
2.00 Max
P
S
Mo
Cu
 
0.045 Max
0.03 Max
0.75 Max
0.50 Max
 

 
SS 310S Chemical Composition, %

Cr
Ni
C
Si
Mn
24.0-26.0
19.2-22.0
0.08 Max
1.50 Max
2.00 Max
P
S
Mo
Cu
 
0.045 Max
0.03 Max
0.75 Max
0.50 Max
 

What are the characteristics of 310/310S Stainless?
  • Oxidation resistance to 2000°F
  • Moderate strength at high temperature
  • Resistance to hot corrosion
  • Strength and toughness at cryogenic temperatures
Typical Applications for 310/310S Stainless
  • Kilns
  • Heat Exchangers
  • Radiant Tubes
  • Muffles, retorts, annealing covers
  • Tube hangers for petroleum refining and steam boilers
  • Coal gasified internal components
  • Staggers
  • Furnace parts, conveyor belts, rollers, oven linings, fans
  • Food processing equipment
  • Cryogenic structures
Fabrication with Stainless 310/310S
Type (S)A240 310S is readily fabricated by standard commercial procedures. In comparison to carbon steel,             stainless steels are tougher and tend to work harden rapidly.
Type (S)A240 310S can be welded using all of the common welding processes.
(S)A240 S31008 Mechanical Properties
Representative Tensile Properties

Temperature, °F
Ultimate Tensile Strength, ksi
0.2% Yield Strength, ksi
Elongation Percent
70
80
35
52
1000
67.8
20.8
47
1200
54.1
20.7
43
1400
35.1
19.3
46
1600
19.1
12.2
48

 
(S)A240 S31008 Typical Creep-Rupture Properties

Temperature, °F
Minimum Creep 0.0001%/hr, ksi
100,000 Hour Rupture Strength, ksi
12000
14.9
14.4
1400
3.3
4.5
1600
1.1
1.5
1800
0.28
0.66

                                                                                                                                                                             
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                   

Tags: SA240 S31008  SA240 TP 310S  S31008 Stainless Plate  TP310S  

0 Comments, 0 Trackbacks