Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS321H,SS321H Stainless plate,SS321H stock,SS321H Supplier (S)A240 S32109, (S)A240 TP 321H, S32109 Stainless Plate, TP321H as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 SS321H,SS321H Stainless plate,SS321H stock,SS321H Supplier
What are Chemical Compositions of A240 SS321H Stainless Steel?
A240 SS321H Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.04-0.10 | 2.00 | 0.045 | 0.030 | 0.75 | 17.0-19.0 |
Ni | Mo | N | Cu | Others | |
9.0-12.0 | | | | Ti: 4×(C+N) min, 0.70 max |
What are Mechanical Properties of A240 SS321H Stainless Steel?
A240 SS321H Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
A240 SS321H | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
0 Comments, 0 Trackbacks