Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS317LN,SS317LN Stainless plate,SS317LN stock,SS317LN Supplier (S)A240 S31753, (S)A240 TP 317LN, S31753 Stainless Plate, TP317LN as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 SS317LN,SS317LN Stainless plate,SS317LN stock,SS317LN Supplier
What are Chemical Compositions of A240 SS317LN Stainless Steel?
A240 SS317LN Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.03 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
11.0-15.0 | 3.00-4.00 | 0.10-0.22 | | |
What are Mechanical Properties of A240 SS317LN Stainless Steel?
A240 SS317LN Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
A240 SS317LN | 550 | 240 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
0 Comments, 0 Trackbacks