Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS316LN,SS316LN Stainless plate,SS316LN stock,SS316LN Supplier (S)A240 S31653, (S)A240 TP 316LN, S31653 Stainless Plate, TP316LN as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Tags:  A240 SS316LN,SS316LN Stainless plate,SS316LN stock,SS316LN Supplier
 
What are Chemical Compositions of A240 SS316LN Stainless Steel?
A240 SS316LN Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.03
2.00
0.045
0.030
0.75
16.0-18.0
Ni
Mo
N
Cu
Others
10.0-14.0
2.00-3.00
0.10-0.16
 
 

What are Mechanical Properties of A240 SS316LN Stainless Steel?
A240 SS316LN Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
A240 SS316LN
515
205
40
95

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 

Tags: A240 SS316LN  SS316LN Stainless plate  SS316LN stock  SS316LN Supplier  

0 Comments, 0 Trackbacks