Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS316H,SS316H Stainless plate,SS316H stock,SS316H Supplier (S)A240 S31609, (S)A240 TP 316H, S31609 Stainless Plate, TP316H as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 SS316H,SS316H Stainless plate,SS316H stock,SS316H Supplier
What are Chemical Compositions of A240 SS316H Stainless Steel?
A240 SS316H Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.04-0.10 | 2.00 | 0.045 | 0.030 | 0.75 | 16.0-18.0 |
Ni | Mo | N | Cu | Others | |
10.0-14.0 | 2.00-3.00 | | | |
What are Mechanical Properties of A240 SS316H Stainless Steel?
A240 SS316H Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
A240 SS316H | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
0 Comments, 0 Trackbacks