Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS304L,SS304L Stainless plate,SS304L stock,SS304L Supplier (S)A240 S30403, (S)A240 TP 304L,S30403 Stainless Plate, TP304L as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 SS304L,SS304L Stainless plate,SS304L stock,SS304L Supplier
What are Chemical Compositions of A240 SS304L Stainless Steel?
A240 SS304L Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.03 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
8.0-12.0 | | 0.10 | | |
What are Mechanical Properties of A240 SS304L Stainless Steel?
A240 SS304L Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
A240 SS304L | 485 | 170 | 40 | 92 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
0 Comments, 0 Trackbacks