Q550C quenched tempered Steel plate

2013年12月11日 by admin

 

Q550C quenched tempered Steel plate, GB/T 16270 Q550C
 
 
GB/T 16270-2009 Q550C High strength structural steel plates in the quenched and tempered condition
Q550C Chemical requirement 

Grade
Chemical requirement or element Max %
 
C
Si
Mn
P
S
Cu
Cr
Ni
Mo
B
V
Nb
Ti
Q550C
0.2
0.8
1.7
0.025
0.015
0.5
1.5
2
0.7
0.005
0.12
0.06
0.05

 
Q550C Property in tensile and yield strength, and impact test requirement

Grade
Property
Impact test
Q550C
Yield Mpa Min
Tensile Mpa
Elongation
Min J
Thickness mm
Thickness mm
Degree
50
50-100
100-150
50
50-100
10-150
%
0
-20
-40
-60
550
530
490
640-820
590-770
16
47
 
 
 

 
HENAN GANG IRON AND STEEL CO.,LTD Supply Q550C in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q550C requirement, please feel free to contact us or email to us by admin@gangsteel.com
 

Tags: Q550C  Q550C quenched tempered Steel plate  GB/T 16270 Q550C  