For more information in LR DH 50 steel grade, please refer to the following:

 
 
LR DH 50 Chemical composition heat analysis
 

Element
LR DH 50 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

 Other alloy elements should be along with LR Society Classification requirement.
     
 
 
 
LR DH 50 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
LR DH 50
8-260
500
610-770
16
33J

Note: the impact energy under less 150mm thickness
 
 
 
 
Related Grade: NV D500 | GL-D550

 