LR AH 42 Steel Plate

2011年11月8日 by admin

LR AH 42 Steel Plate

 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in LR AH 42 steel grade, please refer to the following:

 
 
 
LR AH 42 Chemical composition heat analysis

Element
LR AH 42 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
 
 
 
 
LR AH 42 Mechanical properties,                           longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
GL- A420
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
 
 
 
Related Grade: NV A420 | GL- A460

 