KR AH43 Chemical composition heat analysis

Element
KR AH43 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with KR Society Classification requirement.
 
 
 
 
KR AH43 Mechanical properties,                         longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
KR AH43
8-260
420
530-680
18
28J