KR AH51 STEEL PLATE

 
KR AH51 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in KR A690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
For more information in KR AH51 steel grade, please refer to the following:
 
 
 
 
KR AH51 Chemical composition heat analysis

Element
KR AH51 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with KR Society Classification requirement.
 
 
 
 
KR AH51 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
KR AH51
8-260
500
610-770
16
33J

Note: the impact energy under less 150mm thickness
 
 
 