SPV355,SPV355 JIS G3115,SPV355 steel plate

2011年4月14日 by admin

 

Adopt Standard JIS G3115

Related grades we could supply:

JIS G3115

SPV235

SPV315

SPV355

SPV410

SPV450

SPV490

 

 

 

  

SPV355 steel plate is for pressure vessels for intermediate temperature service in JIS G3115-2000
SPV355 Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

About the detail information of SPV355 is in the following.


SPV355 Chemical composition cast analysis:

Element

SPV355  Max %

C

0.20

Si

0.15-0.55

Mn

1.60

P

0.030

S

0.030

 

SPV355 Mechanical properties:           

Grade

Thickness

Yield Strength

Tensile Strength

(mm)

MPa (min)

MPa

 

 

 

SPV355

≤ 50

355

520-640

50> to ≤100

355

520-640

100> to ≤200

315

520-640

 