SM520C Steel Plate

 

SM520C steel grade is a low carbon, high strength structural steel With this low carbon equivalent, it process good cold forming property. SM520C steel plates usual supplied in normalized or control rolled delivery condition.


SM520C steel grade usual be used in machinery parts, boom, crane, chassis , buildings bridges and mobile equipment.

 

Gangsteel exported SM520C to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM490A/B/C steel grade too. If you any need in SM520C, Please contact Gangsteel to get the competitive price soon.

 

SM520C steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.20
0.20

Product Analysis

1.60

 

Product Analysis

0.55

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

 

SM520C steel grade Tensile Requirements

 

Mechanical Property of SM520C steel grade

SM520C steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm
Elongation under in [16 mm], min, %
Elongation in above [16 mm], min, %

Tensile strength, kis [MPa]

[520-640]

Yield strength, min, kis [MPa]

[365]

[355]

[355]

[325]

[…]

15

21

 

Gangsteel had many stocks in alloy steel of SM520C steel plates. If you need them more stock, please click Gangsteel stock.

For more information in Price and MTC in SM520C steel grade, please contact us by email or calling.

 

SM520C,SM520C steel,SM520C Grade,SM520C steel grade,SM520C steel plate,SM520C grade

 

 

Tags: SM520C  SM520C steel  SM520C Grade  

0 Comments, 0 Trackbacks