SM400C,SM400C steel,SM400C Grade,SM400C steel plate,JIS G3106

2011年4月14日 by admin

SM400C,SM400C steel,SM400C Grade,SM400C steel grade,SM400C steel plate,SM400C

 

Adopt standard: JIS G3106-2004

Grade :SM570,SM520,SM520C,SM520B,SM490YB,SM490YA,

SM490C,SM490A,SM400A,SM400B,SM400C,SM490B steel grade.

 

SM400C Steel Plate

SM400C
Commonly used in the engineering and construction industry, SM400C offers low yield and tensile strength and is supplied with a variety of treatments and test options making it highly usable steel in your construction project. SM400C steel plates usual supplied in control rolled delivery condition.

 

Gangsteel exported SM400C to many largest factory in Korea country and have much experience in Super Thick steel plate in UT S2E3, S1E2 and S0E1 technical to promise the inner quality of steel plate.

 

Besides that, Gangsteel also supply SM400A/B/C, SM490YA/YB, and SM400C/B/C steel grade too. If you any need in SM400C, Please contact Gangsteel to get the competitive price soon.

 

SM400C steel grade Chemical Requirements

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

50mm or under
50mm - 100mm

0.18
0.18

Product Analysis

1.40

 

Product Analysis

0.35

 

 All thick

0.035

Phosphorus

%

 

 

 

 

 

 

All thick

0.035

 

 

 

 

 

 

 

 

SM400C steel grade Tensile Requirements

 

Mechanical Property of SM400C steel grade

SM400C steel grade

Tensile strength, kis [MPa]

8mm-160mm

Yield strength, min, kis [MPa]

8mm-16mm
16mm-40mm
40mm-75mm
75mm-100mm
100mm-160mm
Elongation under in [16 mm], min, %
Elongation above in [16 mm], min, %

Tensile strength, kis [MPa]

[490-610]

Yield strength, min, kis [MPa]

[245]

[235]

[215]

[215]

[205]

18

24

 

Gangsteel had many stocks in alloy steel of SM400C steel plates. If you need them more stock, please click Gangsteel stock.

 

For more information in Price and MTC in SM400C steel grade, please contact us by email or calling.

 