ABS GRADE E general Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

N

ABS GRADE E

0.18

0.1-0.35

0.70

0.035

0.035

0.02

Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

ABS GRADE general strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

ABS GRADE E

mm

Min Mpa

Mpa

Min %

-40

J

J

t≤50

235

400-520

22%

20

27

50t≤70

235

400-520

22%

24

34

70t≤100

235

400-520

22%

27

41

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of ABS GRADE E

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E

GL-E

LR/E

BV/E

CCS/E

K E

R E

RI/E

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

Tags: ABS E  AB/ E  ABS Grade E  ABS Gr E  AB/E steel plate  ABS Grade E supplier  

0 Comments, 0 Trackbacks