New Products /back


07MnCrMoVR|07MnCrMoVR Steel plate|07MnCrMoVR Spherical tanker

2011年9月16日 by admin

07MnCrMoVR LPG Steel plate for Spherical tanker

 
Gangsteel supplies as specialist of 07MnCrMoVR,produces according to standard GB19189&GB 6654,intended particularly for holding 100,000 cubic meters floating roof tanker in Oil Reserve Base.
 
Other Grade: 07MnCrMoVDR
 
Specifications following:
 
1. Thickness*width*length:8-160mm*1500-3900mm*3000-18000mm
 
2. Adopting standards:WYJ036-2005,GB19189,GB6654,JB4730
 
3.Dimensin,shape,weight and allowable deviation according to       standards:GB/T709&GB6654 , ASME SA20/20M
 
4.Supplied in the as-rolled condition: Quench+Temper+S3
 
5.Chemical composition:
 C≤0.09,P≤0.020,S≤0.010,Ni≤0.40,Pcm≤0.20
 
6.Mechanical property:
 Rp0.2(Mpa):≥490MPa,Rm (Mpa)≥610- 730MPa,Elongation rate≥    17%,Yield Ratio≤0.91,Impact Value:-20 AKV≥50J(-20)
 
7.Ultrasonic test: ASTM435/A435M-90 or S12(ASTM A578M-96)
 
8.Delivery time:30-60 days
 
9.Payment term:T/T or L/C
 
10.Minimal order: 1 pcs

 

Tags: 07MnCrMoVR  07MnCrMoVR steel plate  GB/T709  GB 6654  

0 Comments, 0 Trackbacks