GL-F500 Chemical composition heat analysis

Element
GL-F500 Max %
C
0.18
Mn
1.70
Si
0.55
S
0.025
P
0.025
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
      
           
 
 
 
 
GL-F500 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
GL-F500
8-260
500
610-770
16
33J