GL-D620 | GL-D620 STEEL PLATE

2011年11月4日 by admin

GL-D620 STEEL PLATE

 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
 
For more information in GL-D620 steel grade, please refer to the following:

 
 
GL-D620 Chemical composition heat analysis

Element
GL-D620 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
 
 
 
 
 
GL-D620 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
GL-D620
8-260
620
720-890
15
41J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV D620 | BV D690
 