GL-A420 Chemical composition heat analysis

Element
GL-A420 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with GL Society Classification requirement.
 
 
 
 
GL-A420 Mechanical properties,                           longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
GL- A420
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
 
 
 
Related Grade: NV A420 | GL- A460

 

 