EN10028-6 P690QL1 steel plate

2013年9月6日 by admin

P690QL1,P690QL1 steel plate,P690QL1 steel grade,EN10028-6 P690QL1

 

Adopt Standard EN 10028-6

Gang steel Grade: 

P355Q,P355QH,P355QL1,P355QL2,P460Q,P460QH,P460QL1,P460QL2,P500Q,P500QH,P500QL1,P500QL2,P690Q,P690QH,P690QL1,P690QL2

 

P690QL1 Steel plate

P690QL1 steel grade is quenched and tempered steel grade for weldable fine grain pressure purposes.


P690QL1 Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

P…Q means the -20 degree and the impact energy is 27J

P…QH means the -20 temperature quality and the impact energy is 27J
P…QL1 means the -40 temperature quality and the impact energy is 27J

P…QL2 means the -60 temperature quality and the impact energy is 27J 

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P690QL1 Chemical composition cast analysis

Element

P690QL1  Max %

Element

P690QL1 max %

C

0.20

Cr

1.50

Si

0.80

Mo

0.70

Mn

1.70

Cu

0.30

P

0.020

Nb

0.06

S

0.010

Ni

         2.50

N

0.015 

TI

0.05

B

0.005

V

0.12



 

            

P690QL1 Mechanical properties,                     longitudinal min impact energy

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

P690QL1

+QT

≤ 50

690

770-940

14

27

50to ≤100

670

770-940

14

27

100o ≤150

630

720-900

14

27

If you want to find our stock in P690QL1 or inquiry from our gangsteel, please feel free to contact us by email or calling.

P690QL1,P690QL1 steel plate,P690QL1 steel grade,EN10028-6,P690QL1

 

Tags: P690QL1  P690QL1 steel plate  P690QL1 steel grade  EN10028-6  P690QL1  EN 10028-6 P690QL1  P690QL1 steel supplier  P690QL1 price  

0 Comments, 0 Trackbacks