Open/Close


Aug16th

Supply EN 10028-3 P275N,P355N,P460N,P275NH,P355NH,P460NH pressure vessel steel plate

EN 10028-3 steel grade specification is for flat products made of steels for pressure weldable fine grain normalized steel grade in P355N, P355NH, P355NL1, P355NL2, P275NH, P460NH, P460NL1, P460NL2, P275NL1 and P275NL2 steel grade.

Apr14th

P460NL2, P460NL2 steel plate,P460NL2 EN10028-3

P460NL2 steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P460NL1, P460NL1 steel plate,EN10028-3 P460NL1

P460NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P460NH, P460NH steel plate,P460NH EN10028-3

P460NH steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P355NL2, P355NL2 steel plate,EN10028-3 P355NL2.

P355NL2 steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P355NL1, P355NL1 steel plate,EN10028-3 P355NL1

P355NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P355N, P355N steel plate,P355N Grade

P355N steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P355NH, P355NH steel plate,EN10028-3 P355NH.

P355NH steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P275NL2, P275NL2 steel plate,EN10028-3 P275NL2.

P275NL2 steel grade is a normalized, weldable fine grain steels for pressure purposed.

Apr14th

P275NL1, P275NL1 steel plate,P275NL1 Grade,EN10028-3 P275NL1

P275NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed.