New Products /back


S960Q steel plate

2011年3月30日 by admin

S960Q steel plate from Gangsteel

 

Adopt standard: S960Q EN 10025-6

Sell steel grade: S960Q steel plate, S960QL steel plate

 

S960 Steel Grade

S960Q steel is high yield strength structural steels in the quenched and tempered delivery state.

 

 

The symbol S is for structural steel, 960 for the minimum yield strength in thickness under 50mm.

Q mean the delivery condition in quenched and tempered.

S960q steel plate could be through the -20 temperature impact and the energy is 30J.

 

About the S960Q steel weldability General requirements for arc welding of the steels specified shall be as given in EN 1011-2.

 

 

Gangsteel Company could supply S960Q steel plate stickly according to EN10025-6 Standard for our customers. our mill have many years experience in S960q steel manufacturing technique.

 

 

For S960Q steel detail informationplease refer to our mill technical date in following:

 

The Chemical of S960Q is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

S960Q

0.200

0.800

1.700

0.025

0.015

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate in S960q

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S960Q

8mm-50mm

Min 960Mpa

980-1150Mpa

10%

-20

Min 30J

51mm-100mm

Min 910Mpa

920-1000Mpa

10%

-20

Min 30J

101mm-150mm

Min 860Mpa

870-980Mpa

10%

-20

Min 30J



 