S890QL steel plate

2011年3月30日 by admin

S890QL steel plate from Gangsteel

 

Adopt standard:  S890QL steel EN 10025-6

Sell steel grade: S890Q steel plate, S890QL steel plate, S890QL1 steel plate

 

S890QL steel plate

 

S890QL is a high strength and toughness steel in min yield strength 890Mpa thickness under 50mm, -40 temperature impact energy 30J in quenched and tempered delivery station.

 

 

Gangsteel export S890QL EN 10025-6 steel plates directly from our mill. Besides, we also have stock in hand in large thickness of S890QL1 steel.

Gangsteel sincerely hope our customers could come to our mill and factory to inspect our quality and ability in manufacture for our long cooperation.

 

 

About S890QL detail informationplease refer to our mill technical date in following:

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

S890QL

0.200

0.800

1.700

0.020

0.010

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S890QL

8mm-50mm

Min 890Mpa

940-1100Mpa

11%

-40

Min 30J

51mm-100mm

Min 830Mpa

880-1100Mpa

11%

-40

Min 30J

101mm-150mm

Min 800Mpa

820-1000Mpa

11%

-40

Min 30J

 

 

 

 