New Products /back


EN 10025-3 S420N,S420N steel,S420N supplier,S420N steel plate

2013年8月26日 by admin

S420N steel is a good weldability structural steel grade. General requirements for arc welding of the steels specified shall be as given in EN 1011-2.
 
Compare the S355N; S420N steel grade has more yield and tensile strength. The equal grade of S420N is S420M.
 
Gangsteel has much experience in manufacture S420N. we cooperated with wuyang mill of HBIS to produce the max thickness 300mm in electroslag remelting technical. Our advantage is that we could supply goods in the fastest delivery time, even in one plate in usual specification.

 
About S420N steel detail information, please refer to technical date in following.
 
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
S420N
0.200
0.600
1.0-1.7
0.030
0.025
0.020
0.020
0.300
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.550
0.100
0.050
0.800
0.050
0.025
 
 

 
The mechanical properties steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S420N
8mm-100mm
360Map-420Mpa
520-680Mpa
19%
-20
40J
101mm-200mm
330Mpa-360Mpa
500-650Mpa
18%
-20
40J
201mm-250mm
320Mpa-330Mpa
500-650Mpa
18%
-20
40J
The min impact energy is longitudinal energy

 
 
 
For more information in S420N quality certificate or inquiry in competitive official quotation, please contact us by email.
 
 

Tags: EN 10025-3 S420N  s420n  s420n steel  S420N supplier  S420N steel plate  