New Products /back


S275N en10025-3 S275N steel plate

2011年4月5日 by admin

S275N steel plate

Adopt standard: EN 10025-3

Sell steel grade: S275N,S355N,S420N,S460N,S275NL,S355NL,S420NL,S460NL steel plate.

 

S275N/S275NL steel plate

 

S275N/S275NL steel is a hot rolled structural steels, which technical delivery conditions for normalized or normalized rolled in weldable fine grain structural steel grade.

 

S275N steel plate is with specified minimum values of impact energy at temperatures not lower than -20 degree.


S275NL steel plate is with specified minimum values of impact energy at temperatures not lower than -50 degree.
 

Gangsteel could supply S275N/S275NL plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.1 or 3.2.

 

About S275N/S275NL detail informationplease check technical date in following.

 

 

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

S275N/NL

0.180

0.400

0.5-1.5

0.030

0.025

0.050

0.020

0.300

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.550

0.100

0.050

0.300

0.050

0.015

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S275NL

8mm-100mm

235Map-275Mpa

370-510Mpa

24%

-50

27J

101mm-200mm

225Mpa-265Mpa

350-480Mpa

23%

-50

27J

201mm-250mm

205Mpa-225Mpa

350-480Mpa

23%

-50

27J

The min impact energy is longitudinal energy

 

 

 

Our mill sells S275NL and S275N in EN10025-3 standard. If you have any need in this steel grade, please inquiry us soon.

 

 

 

Tags: s275n  en10025 s275n  s275n steel  

0 Comments, 0 Trackbacks