New Products /back


S450J0 EN10025-2 S450J0 steel plate

2011年4月5日 by admin

S450J0,S450J0 steel.s450j0 grade,s450j0 steel plate,s450j0 steel grade,en10025-2,s450j0

 

Adopt standard:  EN10025-2

Sell steel grade: S450J0, S355J2, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355K2

 

S450J0 steel plate

 

 

S450J0 steel plate has a -0 degree temperature steel. Compare with S355J0, and S355J2G3, S450J0 steel plate has a more yield strength in min 450Mpa under thickness of 16mm. In that case, steel grade S450J0 is better in riveted, bolted, or welded construction of bridges and buildings.



Gangsteel is specialized in supplying S450J0 steel grade in super thick steel plate. We exported our goods to Vietnam, Korea and Singapore in this grade in many years. Gangsteel promised that we used our best service to enlarge steel market of oversea.

 

If you need low yield and tensile strength, you could choose S355J0 steel grade Which has min 350Mpa yield strength under thickness of 16mm.

 

For more information S450J0, please refer them in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S450J0

0.23-0.24

0.600

1.800

0.040

0.040

0.027

0.060

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S450J0

8mm-100mm

380Map-450Mpa

550-720Mpa

17%

0

27J

101mm-200mm

380Mpa

530-700Mpa

17%

0

27J

201mm-400mm

17%

0

27J

The min impact energy is longitudinal energy

 

 

Gangsteel had many stocks in carbon steel plate, for S450J0 steel grade, we suggest you to order new goods because this grade is hard to find stock in steel market of China

 

If you have any need in S450J0 steel plate, or S450J0, S355J2, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355K2 steel grade, please feel free to contact us by email or calling.

 

S450J0,S450J0 steel.s450j0 grade,s450j0 steel plate,s450j0 steel grade,en10025-2,s450j0

 

 

 

Tags: s450j0  en10025  s450j0 steel  