New Products /back


EN 10025-2 S275JR high strength structural steel plate

2013年8月28日 by admin

 

Steel Grade: S275JR ( 1.0044)

 

Related grades: S235JRS235J0S235J2S275JRS275J0S275J2S355JRS355J0S355J2, S355K2S450J0S275JRG3

 

S275JR Steel Plates

S275 – a structural grade steel with a minimum yield strength of 275 N/mm² which widely used in the engineering and construction industries.

 

 

S275 offers high yield and tensile strength and is supplied with a variety of treatments and test options to ensure it is a highly usable steel in your various projects.

 

EN 10025-2 S275JR High Yield Strength Structural Steel Plate

S symbol for Structural Steel

JR symbol 20 temperature impact test

J0 syambol 0 temperature impact test

J2 symbol -20 temperature impact test

 

S275JR Characteristic

S275JR is a low carbon, high tensile strength structural steel which can be readily welded to other weldable steel. 

With its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in normalized or controlled rolling condition.

 

S275JR Application 

Structural application in freight cars, transmission towers, dump trucks, cranes, trailers, bull dozers, excavators, forestry machines, railway wagons, dolphins, penstocks, pipes, highway bridges, building structures, oil and gas platforms, offshore structures, shipbuilding, power plant, palm oil equipments and machineries, fans, pumps, lifting equipments and port equipments.

 

Dimension we could supply: 

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

 

S275JR Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, Q+T, N+T, TMCP, Z15, Z25, Z35

 

S275JR Chemical Composition(max %): 

Grade

C%

Si %

Mn %

P %

S %

N %

Cu %

S275JR

0.25

-

1.60

0.045

0.045

0.014

0.60

S275JR Mechanical Properties.

Grade

Thickness (mm)

Min Yield (Mpa)

Tensile (Mpa)

Elongation (%)

Min Impact Energy

S275JR

8mm-100mm

235Mpa-275Mpa

450-630Mpa

21-23%

20

27J

101mm-200mm

205-225Mpa

450-600Mpa

19%

20

27J

201mm-400mm

195-205Mpa

-

-

20

27J

The min impact energy is longitudinal energy

Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in low alloy high strength structural steelmainly dealing with specification standard plates in EN 10025-2, EN 10025-3, EN 10025-4, EN 10025-6, ASTM A633, ASTM A573, ASTM A572, DIN 17100, JIS G3106, ASTM A709, ASTM A283ASTM A529, ASTM A656, EN 10225, ISO 630, NFA 35-501, and so on, the thickness up to 300mm.

To find out more about S275JR or other low alloy high strength steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

 

 

Tags: EN 10025-2 S275JR  S275JR  S275JR steel plate  EN 10025-2 steel plate  EN 10025-2 S275JR  