DNV EH36 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV/EH36

0.18

0.10-0.50

0.9-1.6

0.035

0.035

0.015-0.08

 

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.40

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

DNV EH36 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV/EH36

mm

Min Mpa

Mpa

Min  %

-40

J

J

t≤50

355

490-620

21%

24

34

50t≤70

355

490-620

21%

27

41

70t≤150

355

490-620

21%

34

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV/EH36

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/EH36

R EH36

LR/EH36

BV/EH36

CCS/EH36

K EH36

GL-EH36

RI/EH36

 