A285 Gr.C Steel Plate
2015年12月4日 by admin
A285 Gr.C Steel Plate
1. A285 steel plates are intended for fusion-welded pressure vessels. Plates are normally supplied in the as-rolled condition.
2. If you have any other requirement for steel plate, please feel free to contact us.