Henan Gang iron and steel co., Ltd supply steel grade BV/A, BV/B, BV/D, BV/E, BV/AH36, BV/DH36, BV/EH36, BV/FH36, BV/AH32, BV/DH32, BV/EH32, BV/FH32.

 

 

 

In EH32 steel plate, our mill have more ingot to provide super thick steel plate, our max per weight of plate is above 24.5mt now, max width is 4000mm..

 

EH32 steel grade is lower than FH32 in yield and tensile strength. It is a good material for shipbuilding in deck. EH32 Grade is in -40 impact test of 34J energy. All of thickness of EH32 material need normalize in delivery station.

 

Henan Gang iron and steel co., Ltd supply EH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.


Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for a long steel business.

 

About EH32 detail informationplease check technical date in following.

 

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

 EH32

0.180

0.1-0.5

0.90-1.6

0.035

0.035

0.05-0.10

0.015

0.200

Cu %

Mo %

Nb %

Ni %

Ti %

 

 

 

0.350

0.080

0.02-0.05

0.400

0.020

 

 

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

EH32

8mm-50mm

Min 315Mpa

440-590Mpa

22%

-40

 34J

51mm-70mm

Min 315Mpa

440-590Mpa

22%

-40

 38J

71mm-100mm

Min 315Mpa

440-590Mpa

22%

-40

 46J

The min impact energy is longitudinal energy

 

 

 

Our mill EH32 always be exported to Singapore and Thailand shipyard for shipbuilding.