A572 Grade 55,A572Gr55,A572 Gr 55,steel plate

2011年4月6日 by admin

Steel Category: Low alloy structural steel plate

Adopt standard: ASTM A 572/A 572M-06

 

A572 Grade 42 steel plate,A572 Grade 50 steel plate,A572 Grade 55 steel plate,A572 Grade 60 steel plate,A572 Grade 65 steel plate.

 

A572 Grade 55 steel plates

 

A572 Gr.55 steel plate is high strength low alloy columbium-vanadium structural steel grade. A 572 Gr.55 steel steel plate are intended for riveted, bolted or welded structural.

 

Compare with A572 Gr.50, A 572 Gr55 steel has a more yield and tensile strength in project. If you want to more yield, you could choose A572 Gr60 and A572 Gr70 to use them in your projects.

 

 

Gangsteel applied our mind to service our customers in super thick steel plate for many years. We are through our reputation, quality and service to enlarge our oversea steel market

 

If you have need in A572 Gr.55, we will use the best quality and the fastest delivery time to satisfy your Demand.

For more information of A572 Gr.55, please refer them in following.

 

The Chemical is max composition of heat analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

Ni %

Co %

A572 Gr.55

0.250

0.400

1.350

0.040

0.050

0.060

0.015

0.050

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

 

A572 Grade 55

8mm-50mm

380Mpa

485Mpa

20%

50mm-200mm

380Mpa

485Mpa

17%

The min impact energy is longitudinal energy

 

 

 

If you want to purchase more yield and tensile steel grade, please check steel grade in A572 Grade 60, A572 Grade 70 steel grade.

 

 

About stock in A572 Grade 55, A572 Grade 60, A572 Grade 65 steel plate, they are hard to find in China steel market now, we suggest customers order new goods to promise quality.

 

For more information in A572 Grade 55 quality certificate or inquiry in competitive official quotation, please contact us by email.

 

 

 

Tags: A572Gr55  A572Gr.55  A572 grade 55  

0 Comments, 0 Trackbacks