ASTM A516Gr.55,A516 Gr 55,A516 Grade 55 steel plate

2011年4月14日 by admin

A516 Grade 55 Steel Grade

 

Steel Category: Boiler & pressure vessel steel plate

Adopt standard:  A516 ASTM

Sell steel grade: A516 Grade 55 steel grade, A516 Grade 60 steel grade, A516 Grade 65 steel grade, A516 Grade 70 steel grade

 

A516 Grade 55 steel plate

 

A516 Grade 55 steel grade is used in moderate and lower temperature pressure vessels steel because of the steel material chemical composition and the property in welding.

 

For the reason of excellent notch toughness and weldability of A516 Grade 55, it sells good to large fabricators service in gas & oil plants.

 

As the largest exported in our mill, Gangsteel also have many size in A 516 Grade 70, A 516 Grade 65, A 516 Grade 55 and A 516 Grade 60 steel plate’s stock list. Gangsteel has a long cooperation with company Indonesia boiler factory and endeavored to enlarge our oversea steel market.


Gangsteel promised that we will use our better services , faster delivery time and the best quality to service our customers.

 

Welcome to visit Gangsteel company and our mill in China

 

If you want find more size in stock list, please check our stock list in A 516 Gr.55.

 

About A516 Grade 55 detail informationplease check technical date in following.

 

 

 

The A516 Grade 55 Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

A516 Gr 55

0.18-0.26

0.13-0.45

0.55-1.3

0.035

0.035

 

 

The mechanical properties at A 516 Grade 55 steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

A516 Gr.55

6mm-40mm

205Mpa

380-515Mpa

27%

40mm-100mm

205Mpa

380-515Mpa

23%

The min impact energy is longitudinal energy

 

 

 

If you have any need in A516 Grade 55, please feel free to contact us soon by email or calling. We will reply to you as early as possible.

 

 

 