A516Gr70| A516Gr70 HIC|A516Gr70 N boiler steel plate

2013年8月19日 by admin

A516Gr70 steel is a carbon pressure vessel steel grade for moderate and lower temperature service.

 

A 516Gr70 usual request normalized if thickness above 40mm, if not , Gangsteel usual delivery in hot rolled or control rolled station. A 516 Gr.70+N or A516gr70N mean that steel grade must be normalized in any thickness.

 

Compare with the A 516Gr60, A 516Gr65, and A 516 Gr55, the A516Gr70 steel grade have better property in tensile and yield strength. Gangsteel also supply the Ultrasonic test in thickness in A 435/A435M, A 577/577M and A 578/A578M to promise the perfect quality in long cooperation.

 

Our plates including A516 Gr70 come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

A516Gr70 steel grade is a advantage Gangsteel company, we exported the super thickness steel plate max 135mm in A516Gr70 to Singapore in the best quality. One of our boss is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

About A516Gr70 detail informationplease check technical date in following.

 

 Table 1 The A 516 Grade 70 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

A516Gr70

0.27-0.31

0.13-0.45

0.79-1.3

0.035

0.035

 

Table 2 The mechanical properties at A 516 Grade 70 steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

A516Gr70

6mm-40mm

260Mpa

485-620Mpa

21%

40mm-100mm

260Mpa

485-620Mpa

17%

The min impact energy is longitudinal energy

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about A516 Gr70 or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

 

 

Tags: A516Gr70  A516Gr70 HIC  A516Gr70 N  