A516Gr65 Boiler and Pressure Vessel Steel Plate

 

Related Grade: A516 Grade 60 | A516 Grade 65 | A516 Grade 55| A516 Grade 70

 

A516Gr65 steel is a carbon pressure vessel steel grade for moderate and lower temperature service for a variety of applications in the Petrochemical, Chemical, Oil & Gas Industries

 

A516Gr65 usual request normalized if thickness above 40mm, if not, Gangsteel usual delivery in hot rolled or control rolled station. A 516 Gr.65+N or A516gr65N mean that steel grade must be normalized in any thickness.

 

Gangsteel also supply the Ultrasonic test in thickness in A435/A435M, A 577/577M and A 578/A578M to promise the perfect quality in long cooperation.

 

Our plates including A516 Gr65 come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

One of our boss is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

Dimension available to us:

Thickness: 6MM to 300MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm

 

The A 516 Grade 65 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

A516Gr65

0.24-0.29

0.13-0.45

0.79-1.3

0.035

0.035

 

The mechanical properties at A 516Gr65 steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

A516Gr70

6mm-40mm

240Mpa

450-585Mpa

23%

40mm-100mm

240Mpa

450-585Mpa

19%

The min impact energy is longitudinal energy

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about A516 Gr65 or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.  

Tags: A516Gr65  A516Gr65 n  A516Gr65 hic  A516 Grade 65  A516 GR65  ASTM A516 Gr65  ASME SA516 Gr65  A516 Gr65 price  

0 Comments, 0 Trackbacks