A516Gr60|A516Gr60 N|A516Gr60 HIC Boiler steel plate

2013年8月19日 by admin

A516Gr60 steel grade is used in moderate and lower temperature pressure vessels steel because of the steel material chemical composition and the property in welding.

 

For the reason of excellent notch toughness and weldability of A516 Grade 60, it sells good to large fabricators service in gas & oil plants.

 

As the largest exported in our mill, Gangsteel also have A516 Grade 70, A516 Grade 65, and A516 Grade 60 steel plate stock list. Gangsteel has long cooperated company in Indonesia boiler factory and endeavored to enlarge our oversea steel market.


Gangsteel promise that we will use our better service , faster delivery time and the best quality to service our customers.Welcome to visit Gangsteel company and our mill in China

 

If you need stock size, please check our stock list in A516Gr60 grade.

About A516Gr60 detail informationplease check technical date in following.

 

The A 516 Grade 60 Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

A516Gr60

0.21-0.27

0.13-0.45

0.55-1.3

0.035

0.035

 

The mechanical properties at A 516 Grade 60 steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

 

A516Gr60

6mm-40mm

 

220Mpa

 

415-550Mpa

25%

40mm-100mm

 

220Mpa

 

415-550Mpa

21%

The min impact energy is longitudinal energy

 

 

 