Supply A302 GRA,A302 GRB,A302 GRC,A302 GRD boiler and pressure steel plate
2013年8月16日 by admin
A302 steel plates standard specification for pressure vessel plates in alloy steel, manganese molybdenum and manganese-molybdenum-nickel.
1. Steel Grade: A302 Grade A, A302 Grade B, A302 Grade C, A302 Grade D
2. Steel Dimension: Thickness: 6-300mm, Width: 1500-4050mm, Length: 3000-15000mm
3. Adopt Standard: ASTM A302 and ASME SA302
4. Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, TMCP, Z15, Z25, Z35
5. Delivery Time: 30days
6. Payment Item: L/C, TT
7. Trade Terms: FOB, CFR or CIF
8. Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, HIC, NACE, and so on.
9. Certificate: ABS, DNV, BV, LR, GL, CSS, KR, NK,RINA, TUV, CE, ISO, and so on.
Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in supplying boiler and pressure vessel steel plate, dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A202, ASTM A203, ASTM A204, ASTM A302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and so on, the thickness up to 300mm.
Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company. We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.
Yours sincerely,
MS. Olina
Tel: 86-0371-88884766 Fax: 86-0371-88884766
Cell: 86-15226033579
Email: olina@gangsteel.com
Skype: gangsteel18
MSN: gangsteel18@hotmail.com
Tags: A302GrA A302GrB A302GrC A302GrD
0 Comments, 0 Trackbacks