New Products /back


A283 Grade B,A283GrB, A283Gr.B,A283 Grade B steel,A283 Gr B steel plate

2011年4月10日 by admin

A283 Grade B,A283GrB, A283Gr.B,A283 Grade B steel,A283 Gr B steel plate

 Adopt standard: ASTM A283/A283M

Gangsteel grade: A283 Grade A, A283 Grade B,A283 Grade C,A283 Grade D
,A283GrA, A283GrB,A283GrC,A283GrD,steel grade.


A283 Grade B steel plate

 

A283 Grade B steel plates furnished shall conform to the requirements of the current of specification a6/a6m. In the process, A283 Grade B shall be made by one or more of following processes: open hearth, basic oxygen or electric furnace.

A283 steel grade covers four grades in A283 Grade A, A283 Grade B, A283 Grade C, and A283 Grade D of carbon steel plates of structural quality for general application

Gangsteel supply A283 Grade B the low and intermediate tensile strength carbon steel to export oversea market, our advantage is to supply super thick steel plate for our customers in the best quality and we also could let the third party to inspect our goods in our mill, for example, GL, DNV, TUV, CE,LR, BV and so on.
 

For more property in A283 Grade B steel plate, please check them in following;

 

 

A283 Grade B steel plate Chemical composition

 

Carbon, max

%

Manganese, max

%

Silicon, max

%

All Thickness

0.17

Product Analysis

0.90

Product Analysis

0.15-0.40

Phosphorus max

%

Sulfur max

%

Copper min %

 

All thickness

0.035

All thickness

0.04

0.20

 

             

 

A283 Grade B steel plate mechanical property

 

Mechanical Property

A283 Grade B

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

 

50-56[345-450]
27[185]

25

28

 

 

 

If you have any need in steel plates of A283 Grade B or order new goods from Gangsteel, please contact us soon by email or calling to us.

 

A283 Grade B,A283GrB, A283Gr.B,A283 Grade B steel,A283 Gr B steel. plate

 

 

 

Tags: A283 Grade B  A283GrB  A283Gr.B  A283 Grade B steel  A283 Gr B steel plate  

0 Comments, 0 Trackbacks