A203 Grade B,A203Gr.B,A203 Gr B,steel plate

2011年4月14日 by admin

Pressure steel plate,A203-Grade-B,A203Grade B,A203 grade B,A203 Gr B,A203GrB,A203 Grade B steel,A203 Gr B steel plate.

 

Adopt standard: ASTM A 203/A 203M-01

Gangsteel steel grade: A203 Grade A,A203 Grade B,A203 Grade D,A203 Grade E and A203 Grade F steel.

 

A203 Grade B steel plate

 

 

A203 Grade B steel grade is a nickel alloy steel plate in welded pressure vessels. For this A 203Grade B is max thickness in 150mm and the element of nickel is 2.25% to be used in manufacturing pressure vessel and boilers.

 

A203 Grade B yield and tensile strength is higher little than A203 Grade A.

 

Gangsteel has a large advantage in pressure vessel and boilers steel plates, not only in technical of steel , but also in the relation with mill. One of boss of Gangsteel is the sales managers who controlled the cost price in mill to give the competitive price to our customers.

Besides that, Gangsteel has a specialized person who worked at production line of steel, to arrange our customer goods to produce as early as possible. Gangsteel welcomes our customer to visit in our mill.

 

A203 Grade B steel Chemical Requirements In product analysis under 50mm

Element

A203 Grade A  Max %

C

0.21

Si

0.13-0.45

Mn

0.78-0.88

P

0.035

S

0.035

Ni

3.18-3.82

 

 

 

A203 Grade B steel Tensile Requirements

Mechanical Property of A203 Grade B steel plate

A203 Grade B

Tensile strength, kis [MPa]

50mm or under

Over 50mm

Yield strength, min, kis [MPa]

50mm or under

Over 50mm
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

Tensile strength, kis [MPa]

70-90 [485-620]
70-90 [485-620]

Yield strength, min, kis [MPa]

40 [275]

40 [275]

17

21

 

If you have any need in A203 Grade B, please contact Gangsteel soon by email or calling.