Adopt Standard: ASME SA514

ASME SA514 Gr.B steel grade


SA514 Gr.B is for high yield strength, quenched and tempered alloy steel plate of structural quality and under intended primarily for use in welded bridges and other structures.

 

 in the heat treatment,SA514 Gr.B shall be heat treatment by the mill to conform to the tensile and hardness requirements by heating to not less 900 degree and quenching in water or oil, tempering at not less 620 degree.

 

Gangsteel is the large agent in HBIS Wuyang mill and we have exported SA514 Gr.B to be used in oil platform project.
If any need in SA514 Gr.B, please feel free to contact us.


SA514 Gr.B steel Chemical requirement in Heat analysis

C %

Mn %

P %

S %

SI %

Ni %

Cr %

0.12-0.21

0.70-1.00

0.035

0.035

0.20-0.35

 

0.40-0.65

Mo %

B %

V %

Ti %

Zr %

Cu %

Co %

0.15-0.25

 

0.03-0.08

0.01-0.03

 

 

 



 

 

Mechanical Property SA514 Gr.B

SA517 Grade B

20mm and under

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]

Elongation in under [50mm], min, %

Brinell Hardness Number

20mm-32mm

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %

20mm and under

760-895

690

18

235-293

20mm-65mm

760-895

690

18



 

 Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate


Equivalent steel grade of SA514 grade B

EN 10149-2

SEW 092

NFA 36-231

S700MC

QStE 690 TM

E 690 D


Related Grade: SA514 grade A| SA514 grade B | SA514 grade C| SA514 grade E| SA514 grade F| SA514 grade H| SA514 grade J| SA514 grade K| SA514 grade M| SA514 grade P| SA514 grade Q| SA514 grade R| SA514 grade S| SA514 grade T

If you want to know price in SA514 Gr.B from Gangsteel, please inquiry us by email or calling to us, we will give our official quotation to you soon.

Tags: SA514 Gr.B  SA514 Grade B  ASME SA514 Gr.B  SA514 Gr.B steel  SA514 Gr.B Supplier  

0 Comments, 0 Trackbacks