New Products /back


SA302 Gr.A,SA302 Gr.A steel,SA302 Gr.A steel plate

2011年6月10日 by admin

SA302 Gr.A,SA302 Gr.A steel,SA302 Gr.A steel plate

 

Adopt standard: ASME SA302

Sell steel grade: SA302 Grade A, SA302 Grade B, SA302 Grade C, SA302 Gr.D steel grade

 

 

SA302 Gr.A steel plates standard specification for pressure vessel plates in alloy steel, manganese molybdenum and manganese-molybdenum-nickel.

 

SA302 Gr.A steel grade is min yield strength in 310Mpa. Gangsteel also supply the Ultrasonic test in thickness in A435/A435M, A577/577M and A578/A578M to promise the perfect quality in long cooperation.

 

Our plates including SA302 Grade A come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

Gangsteel supplied SA302 Gr.A to export many years. We have contacted the technical department of wuyang mill, from ingot or billet steel, to hot rolled process and normalized treatment, each item in manufacture, Gangsteel have the person to tract for our customers in order to in the fastest delivery time.

 

SA302 Gr.A steel Chemical Requirements:

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

25mm or under
25mm - 50mm
over 50mm

0.20
0.23
0.25

Heat Analysis

Product Analysis

0.95-1.30
0.87-1.41


Heat Analysis

Product Analysis

0.15-0.40

0.13-0.45

 

All thick

 

0.035

 

 

Molybdenum max

%

Nickel  max

%

Phosphorus

%

 

 

Heat Analysis

Product Analysis

0.45-0.60

0.41-0.64

Heat Analysis

Product Analysis

…..

……

All thick

0.035

 

SA302 Gr.A steel Tensile Requirements:

Mechanical Property of SA302 Gr.A steel plate

SA302 Gr.A

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

75-95 [515-655]
45 [310]

15

19

 

If you have any need in SA302 Gr.A steel, please feel free to CLICK HERE to contact us soon by email or calling.

Tags: SA302 Gr.A  SA302 Grade A  SA302 Gr.A steel  SA302 Gr.A steel plate  