ABS GRADE D STEEL PLATE
2013年8月23日 by admin
Gangsteel is specialized in supplying ABS general strength steel plate in ABS Grade D. For more information of Grade D steel plate, please check them in following:
ABS GRADE D general Strength Chemical Composition | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
ABS GRADE D | 0.21 | 0.35 | 0.80 | 0.035 | 0.035 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
ABS GRADE D general strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
ABS GRADE D | mm | Min Mpa | Mpa | Min % | -20 | J | J |
t≤50 | 235 | 400-520 | 18% | 20 | 27 | ||
50<t≤70 | 235 | 400-520 | 18% | 24 | 34 | ||
70<t≤100 | 235 | 400-520 | 18% | 27 | 41 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of ABS GRADE D | |||||||
NV D | GL-D | LR/D | NV/D | CCS/D | K D | R D | RI/D |
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.