AB/DH32|ABS DH32 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade DH32. For more information of GradeDH32 steel plate, please check them in following:
AB/DH32 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
AB/D32 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | - |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/DH32 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
AB/DH32 | mm | Min Mpa | Mpa | Min % | -20 | J | J |
t≤50 | 315 | 440-590 | 22% | 22 | 31 | ||
50<t≤70 | 315 | 440-590 | 22% | 26 | 38 | ||
70<t≤100 | 315 | 440-590 | 22% | 31 | 46 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/DH32 | |||||||
NV D32 | GL-D32 | LR/DH32 | BV/DH32 | CCS/D32 | K D32 | R D32 | RI/D32 |