ASTM A662 Grade B STEEL PLATE
2013年7月15日 by admin
ASTM A662 standard specification for pressure vessel plates, carbon-manganese-silicon steel, for moderate and lower temperature service
ASTM A662 plates over
Our plates including A662 Grade B come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.
Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1 | S5 | S6 | S8 | S9 | S11 | S12 |S17
Dimension: Thickness:
Width:
Length:
ASTM A662 Grade B Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
A662 Grade B | 0,22 | 0.13-0.45 | 0.79-1.62 | 0,035 | 0,035 | | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
| | | | | | |
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Grade | ASTM A662 Grade B Mechanical Property | |||
Thickness | Yield | Tensile | Elongation | |
A662 Grade B | mm | Min Mpa | Mpa | Min % |
6-50 | 275 | 450-585 | 23% | |
50-200 | 275 | 450-585 | 20% |
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
Related Grade: A662 Grade A| A662 Grade C
Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A662, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A285, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.
To find out more about A662 Gr.B or other boiler and pressure vessel steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.
0 Comments, 0 Trackbacks