Steel Category: Low alloy structural steel plate
Adopt standard: A 573/ A 573M-05
Sell steel grade: A573 Grade 58, A573 Grade 65,A 573 Grade 70 steel plate
 
 
A573 Grade 58 steel plate
 
 
A573 Gr. 58 steel is a improved toughness carbon steel plate. The upper limit of manganese for Gr.58 may be exceeded, provided that the carbon content plus 1/6 manganese content does not exceed 0.40% based on heat analysis.

 
If you need more yield and tensile in A573 specification, you could choose our steel grade in A 573 Gr.65 and A 573 Gr.70.

 
Gangsteel always exported that A573 Gr.58 steel plate to Jordan and middle of East Europe country for structural building in bridge and skyscraper.
 
Gangsteel sincerely hope old and new customers visit our mill to contact our long steel business in order to enlarge our oversea steel market.
 
About A573 Gr.58 steel grade more property, please refer to them in following:
 
 
Table for Chemical list:
 

Grade
C %
Si %
Mn %
P %
S %
A573 Gr.58
0.230
0.10-0.35
0.6-0.9
0.035
0.040

 
 
 
Table for yield and tensile strength lsit:
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
A573 Gr.58
6mm-40mm
220Mpa
400-490Mpa
24%
40mm-100mm
The min impact energy is longitudinal energy

 
 
About the stock specification, because Gangsteel exported all of goods which we ordered for our customers, so we do not have stock goods in A573 Grade 58, A573 Grade 65 and A573 Grade 70.

If you need A573 Gr. 58 steel plates, Gangsteel suggest you order them in our mill.
 