New Products /back


ABS AH32,ABS Grade AH32,AB AH32,steel

2011年3月15日 by admin

 

AB/AH32,ABS AH32,Grade AH32,AH32 steel,AB/AH32 steel ,AH32 steel
 
 
Henan Gang iron and steel co., Ltd supply steel grade AB/AH36, AB/DH36, AB/EH36, AB/FH36, AB/AH32, AB/DH32, AB/EH32, AB/FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. AB/AH40, AB/DH40, AB/EH40, AB/FH40.
 
AH32 must normalize in each thickness compare with Grade D. For example ABS A, ABS B, ABS D, and ABS E are the ordinary strength in ABS Classification Society.  
 
AH32 steel plate usual be used in the main structural build including the bull and oil platform.
Our mill could produce size in the following:

Thickness: 6mm to 220mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
 
Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 220mm which beyond nine classification society approval.
Henan Gang iron and steel co., Ltd has two large warehouse stock in shanghai port and tianjin port, we have stock in AH36, DH36, EH36, grade D , grade E and steel Coil in Grade A, grade B from thickness 5mm to 18mm in various specification and Classification Society.
 
 
If you want order news goods from mill, we could give our mill competitive price for our long business in steel plates. We sincerely hope old and new customers to visit our mill for a long steel business
 
About AH32 detail information,please refer to technical date in following.
The Chemical is max composition of product analysis:
 
 

Grade
C %
Si %
Mn %
P %
S %
AH32
0.180
0.10-0.35
0.700
0.035
0.035

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
AH32
8mm-50mm
Min 315Mpa
440-590Mpa
22%
0
34J
51mm-70mm
Min 315Mpa
440-590Mpa
22%
0
38J
71mm-100mm
Min 315Mpa
440-590Mpa
22%
0
46J
The min impact energy is longitudinal energy

 
 
 
If you have any need DNV AH32, BV AH32, ABS AH32, LR AH32, GL AH32, RINA AH32, NK AH32 steel plate, please feel free to contact us.
 
AB/EH32,ABS AH32,AH32,AH32 steel,AB/AH32 steel plate, AH32 grade
 
 

Tags: ABS AH32  ABS Grade AH32  AB AH32  

0 Comments, 0 Trackbacks