Q960E quenched tempered Steel plate, GB/T 16270 Q960E
2013年12月26日 by admin
Q960E quenched tempered Steel plate, GB/T 16270 Q960E
GB/T 16270-2009 Q960E High strength structural steel plates in the quenched and tempered condition
Q960E Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q960E | 0.2 | 0.8 | 1.7 | 0.020 | 0.010 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q960E Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q960E | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 100-150 | % | 0 | -20 | -40 | -60 | |
960 | - | - | 980-1150 | - | 10 | | | 27 | |
HENAN GANG IRON AND STEEL CO.,LTD Supply Q960E in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q960E requirement, please feel free to contact us or email to us by admin@gangsteel.com