Q890E quenched tempered Steel plate, GB/T 16270 Q890E
2013年12月26日 by admin
Q890E quenched tempered Steel plate, GB/T 16270 Q890E
GB/T 16270-2009 Q890E High strength structural steel plates in the quenched and tempered condition
Q890E Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q890E | 0.2 | 0.8 | 1.7 | 0.020 | 0.010 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q890E Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q890E | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 100-150 | % | 0 | -20 | -40 | -60 | |
890 | 830 | - | 940-1100 | - | 11 | | | 27 | |
HENAN GANG IRON AND STEEL CO.,LTD Supply Q890E in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q890E requirement, please feel free to contact us or email to us by admin@gangsteel.com