New Products /back


AQ43,ABS AQ43,AB/AQ43,AB/AQ43 ship plate

2011年4月9日 by admin

AQ43,ABS AQ43,AB/AQ43,AB/AQ43 ship plate

 

Related mill: HBIS (heibei iron & steel co.,ltd),Wisco (wuhan iron and steel group),Shougang mill (shougang group), Xinyu mill (xinyu iron & steel co., ltd),Baosteel (Baosteel group co.,ltd)

 

Keyword:AQ43,ABS AQ43,AB/AH43,AB/AH43 ship steel,AQ43 steel,AQ43 price,AQ43 steel plate, abs grade AQ43.

ABS Grade AQ43 Detail productive technology in the following:

 

1.       Adopt standard: ABS (American Bureau of shipping)

2.       AQ43 application fields:
AQ43 is a super high strength quenched and tempered steel grade. It used in offshore drilling platform, Shipping marine engineering and Hull Structural project.

3.       AQ43 Chemical composition:

 

Grade

C % max

Si % max

Mn % max

P % max

S % max

AB/AQ43

0.21

0.55

1.7

0.035

0.035

 

4.       AQ43 Mechanical Property:

  

Grade

Yield Strength

Tensile Strength

Elongation

Impact Energy

ABS AQ43

MPa (min)

MPa

% (min)

0 degree J

AB/AQ43

 420

530-680

18

41

 

5.       Heat Treatment: Quenched and tempered


6.  Tolerance: The thickness tolerance is -+0.03mm


7.  Size: Thick: 8mm-180mm, width: 1500mm-4000mm, length: 3000mm-18000mm

 

8.        Delivery time: 40-45days

 

Gangsteel has much experience in super high strength hull structural steel plate, if you have any need in ABS/AQ43 steel plate; please feel free to contact us. We will give our mill competitive price on the base of faster delivery.

 

Other super strength steel grade in Gangsteel:

AB/AQ43,AB/DQ43,AB/EQ43,AB/AQ47,AB/DQ47,AB/EQ47,AB/AQ51,AB/DQ51,AB/EQ51,AB/AQ56,AB/DQ56,AB/EQ56,AB/AQ63,AB/DQ63,AB/EQ63,AB/AQ70,AB/DQ70,AB/EQ70

 

 

 

 